TM 55-1945-205-24-20283 00 30283 00a.Create templates from Kraft paper starting with a size outside the prepared area and making progressively smaller ones to equal the thickness of the laminate being repaired.b.Cut fiberglass cloth pieces with scissors to equal the templates.c.Clean the prepared area with a wiping rag soaked in acetone.WARNINGNOTEAfter mixing, the resin with hardener can be used for approximately 20 - 30 minutes.d.Mix hardener into the resin can.e.Lay out a sheet of polyethylene cellophane (separating film), larger than the largest piece of fiberglass cloth, on a horizontal surface.f.Place the largest piece of fiberglass on the film.TRANSOM1, 2 and 3Gelcoat1 oz. Mat2 Units¾ in. Plywood1½ oz. Mat¾ in. Plywood4½ oz. Mat2 Units1 oz. MatGelcoatDECK HORIZONTAL SURFACE1, 2 and 3Gelcoat1 oz. Mat1 UnitSyntactic Foam5/8 in. Plywood1 UnitLay-Out Schedule Notes11 Unit shall be 1 oz. Mat and 18 oz. Woven Roving.2Syntactic Foam: 1 part Milled Fibre, 2 parts Resin, 3 parts Glass Bubbles. Thicken as required with Milled Fibre.3Resin shall be polyester isopthalic in hull and orthopthalic in deck and transom.Table 1. Lay-Out Details. (Continued)AREANOTESLAY-OUT
Integrated Publishing, Inc. - A (SDVOSB) Service Disabled Veteran Owned Small Business