TM 55-1945-205-24-20284 00 30284 00a.Create templates from Kraft paper starting with a size outside the prepared area and making progressively smaller ones to equal thickness of laminate being repaired.b.Cut glass cloth pieces with scissors to equal templates.c.Clean the prepared area with a wiping rag soaked in acetone.NOTEAfter mixing, the resin with hardener can be used for approximately 20 - 30 minutes.d.Mix hardener into the resin can.e.Lay out a sheet of polyethylene cellophane (separating film), larger than the largest piece of fiberglass cloth, on a horizontal surface.f.Place largest piece of fiberglass on film.g.Apply mixed resin on the fiberglass cloth using a putty knife.h.Center next largest piece of fiberglass cloth on top of first piece and apply as little resin as possible on second cloth.i.Using putty knife, work the resin into patch until it becomes clear and without white patches, which indicates areas that are not saturated sufficiently with resin.TRANSOM1, 2 and 3Gelcoat1 oz. Mat2 Units¾ in. Plywood1½ oz. Mat¾ in. Plywood4½ oz. Mat2 Units1 oz. MatGelcoatDECK HORIZONTAL SURFACE1, 2 and 3Gelcoat1 oz. Mat1 UnitSyntactic Foam5/8 in. Plywood1 UnitLay-Out Schedule Notes11 Unit shall be 1 oz. Mat and 18 oz. Woven Roving.2Syntactic Foam: 1 part Milled Fibre, 2 parts Resin, 3 parts Glass Bubbles. Thicken as required with Milled Fibre.3Resin shall be polyester isopthalic in hull and orthopthalic in deck and transom.Table 1. Lay-Out Details.AREANOTESLAY-OUT
Integrated Publishing, Inc. - A (SDVOSB) Service Disabled Veteran Owned Small Business